Compositions: ceramic – Ceramic compositions – Refractory
Patent
1997-09-30
1999-12-14
Group, Karl
Compositions: ceramic
Ceramic compositions
Refractory
501 87, 501 961, 501 963, 264668, C04B 355835
Patent
active
060017570
ABSTRACT:
A hard sintered body for a tool contains 25 to 47 vol. % of cBN, 40 to 70 vol. % and especially less than 45 vol. % in total of a carbo-nitride, and a boride of Ti, and 2 to 20 vol. % in total of a boride and a nitride of Al. In the carbo-nitride of Ti, the ratio of carbon to nitrogen is in the range of 60:40 to 30:70. In this hard sintered body, cBN particles are bonded to each other through binder phases. The obtained hard sintered body for a tool is excellent in wear resistance and chipping resistance for high-speed cutting of hardened steel.
REFERENCES:
patent: 4334928 (1982-06-01), Hara et al.
patent: 5092920 (1992-03-01), Nakai et al.
patent: 5200372 (1993-04-01), Kuroyama et al.
patent: 5288297 (1994-02-01), Ringwood
patent: 5326380 (1994-07-01), Yao et al.
patent: 5328875 (1994-07-01), Ueda et al.
patent: 5466642 (1995-11-01), Tajima et al.
patent: 5569862 (1996-10-01), Kuroyama et al.
Fukaya Tomohiro
Nakai Tetsuo
Fasse W. F.
Fasse W. G.
Group Karl
Sumitomo Electric Industries Ltd.
LandOfFree
Hard sintered body for tool does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Hard sintered body for tool, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Hard sintered body for tool will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-863164