ABSTRACT:
Coke intended for use in graphitized articles such as graphite electrodes is thermally desulfurized and made more ordered by heating in the absence of air at a temperature between about 1600.degree. C and 2200.degree. C for a period of at least one hour before the particles are mixed with binder. Coke processed in this manner yields graphite electrodes of superior flexural strength and having lower coefficients of thermal expansion.
REFERENCES:
patent: 3369871 (1968-02-01), Hardy et al.
patent: 3506745 (1970-04-01), Juel et al.
patent: 3853793 (1974-12-01), Brown et al.
Merrow Jack Kenneth
Moore Arthur William
Volk Herbert Franz
Evans J. Hart
Padgett Benjamin R.
Parr E. Suzanne
Union Carbide Corporation
LandOfFree
Graphite electrode and method of making does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Graphite electrode and method of making, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Graphite electrode and method of making will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1549513