ABSTRACT:
A method for forming nickel base superalloy articles of manufacture by a combination of hot die forging, isothermal forging and heat treatment below and above the solvus.

REFERENCES:
patent: 4612062 (1986-09-01), Nazmy et al.
patent: 4685977 (1987-08-01), Chang
patent: 5061324 (1991-10-01), Chang
patent: 5143563 (1992-09-01), Krueger et al.
patent: 5413752 (1995-05-01), Kissinger et al.
patent: 5529643 (1996-06-01), Yoon et al.
patent: 5547523 (1996-08-01), Blankenship et al.
Metals Handbook, 9th ed, vol. 14 "Isothermal and Hot Die Forging" pp. 150-157, 1988. TA 459 M 143 in STIC.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Grain size control in nickel base superalloys does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Grain size control in nickel base superalloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Grain size control in nickel base superalloys will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1454899

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.