Glass compression seals using low temperature glass

Joints and connections – Utilizing thermal characteristic – e.g. – expansion or...

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

403404, 403179, 65 5931, 65 5932, 174152GM, C03C 2708

Patent

active

046783580

ABSTRACT:
A metal housing is provided with lead in members by way of a compression seal using a glass that can be worked below about 480.degree. C. The housing and lead in members can be preplated in a low cost process to provide a suitable protective coating that is present under the glass after the seal is made. This obviates a post seal plating and therefore avoids the related problems. It also permits using aluminum as the housing material.

REFERENCES:
patent: 2770923 (1956-11-01), Dalton et al.
patent: 3188720 (1965-06-01), Husni
patent: 3302961 (1967-02-01), Franklin
patent: 3370874 (1968-02-01), Scherer et al.
patent: 3685005 (1972-08-01), D'Alessandro
patent: 4029897 (1977-06-01), Mayer et al.
patent: 4128697 (1978-12-01), Simpson
patent: 4417913 (1983-11-01), Davis et al.
patent: 4430376 (1984-02-01), Box

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Glass compression seals using low temperature glass does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Glass compression seals using low temperature glass, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Glass compression seals using low temperature glass will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1659819

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.