Glass compositions for ceramic electrolyte electrochemical...

Compositions: ceramic – Ceramic compositions – Devitrified glass-ceramics

Reexamination Certificate

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

C501S015000, C501S017000, C501S021000, C501S032000, C501S072000

Reexamination Certificate

active

06878651

ABSTRACT:
A glass composition consisting essentially by mol percent of about 55<SiO2<75; 5<BaO<30; and 2 <MgO<22 for use as a matrix of composite materials. A method of making a glass matrix-ceramic particulate composition useful for sealing electrochemical structures, such as solid oxide fuel cells is also disclosed. Method steps include the admixture of finely divided Mg2SiO4particulates with the matrix glass, to reach an overall composition by mol percent of about 55<SiO2<65; 5<BaO<15; and 25<MgO<35.

REFERENCES:
patent: 3022179 (1962-02-01), Morrissey
patent: 3489627 (1970-01-01), Botden et al.
patent: 3501322 (1970-03-01), Dumbaugh et al.
patent: 3839055 (1974-10-01), Grossman
patent: 3935017 (1976-01-01), Gardner
patent: 4687749 (1987-08-01), Beall
patent: 4746578 (1988-05-01), Kondo et al.
patent: 4806334 (1989-02-01), Fujinaka et al.
patent: 4827606 (1989-05-01), Szreders et al.
patent: 4935387 (1990-06-01), Beall et al.
patent: 4948758 (1990-08-01), Becall et al.
patent: 4949010 (1990-08-01), Petersen et al.
patent: 5091345 (1992-02-01), Becker
patent: 5284807 (1994-02-01), Komori et al.
patent: 5501914 (1996-03-01), Satake et al.
patent: 5525855 (1996-06-01), Gotoh et al.
patent: 5827620 (1998-10-01), Kendall
patent: 6099985 (2000-08-01), Elangovan et al.
patent: 6271158 (2001-08-01), Xue et al.
patent: 6291092 (2001-09-01), Kohli et al.
patent: 6296963 (2001-10-01), Nanjo
patent: 6430966 (2002-08-01), Meinhardt et al.
patent: 6532769 (2003-03-01), Meinhardt et al.
patent: 0982274 (1999-07-01), None
patent: 1008563 (1999-12-01), None
patent: 1010675 (1999-12-01), None
patent: 1008563 (2000-06-01), None
patent: 1010675 (2000-06-01), None
patent: 50008442 (1975-04-01), None
patent: WO 9846540 (1998-10-01), None
Aluminosilicate Glass Ceramics as Sealant in Sofc Stacks; by: N. Lahl, L. Singheiser, and K. Hilpert; Institute for Materials and Processes in Energy Technology, Research Center Jülich 52424 Jülich, Germany; Electrochemical Society Proceedings vol. 99-10; pp. 1057-1066, No Date Available.
Glass-Ceramic Sealants for Solid Oxide Fuel Cells: Part I. Physical Properties; by K.L. Ley, M. Krumpelt, R. Kumar, J.H. Meiser, and I. Bloom; Electrochemicial Technology Program, Chemical Technology Division, Agronne National Laboratory, Argonne, Illinois; J. Mater, Res. vol. 11, No. 6, Jun. 1996;; pp. 1489-1493.
The American Ceramic Society, Annual Meeting Abstracts, 102ndAnnual Meeting & Exposition Apr. 30-May 3, 2000, St. Louis, MO, “Processing Methods for Ceramic Joining”, 1 pp.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Glass compositions for ceramic electrolyte electrochemical... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Glass compositions for ceramic electrolyte electrochemical..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Glass compositions for ceramic electrolyte electrochemical... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-3384266

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.