ABSTRACT:
A coating composition of an alkoxy silane reacted with the surface of a glass substrate and a cleaning composition and method for cleaning said glass area is disclosed. The coating provides water repellency, durability and ease of cleaning to a glass or other siliceous surface. The coating is formed by applying an excess of an alkoxy solution containing a sulfuric acid to a glass surface with an excess of solution being applied. Preparatory to such coating application, the glass, especially if its surface is a weathered (non-virgin) surface, is cleaned vigorously with a cleaning solution containing water, phosphoric acid, hydrofluoric acid and sulfuric acid.
REFERENCES:
patent: 2612458 (1952-09-01), Stedman
patent: 2923653 (1960-02-01), Matlin et al.
patent: 2962390 (1960-11-01), Fain et al.
patent: 3104167 (1963-09-01), Cotteta
patent: 3244541 (1966-04-01), Fain
patent: 3442664 (1969-05-01), Heine
patent: 3448055 (1969-06-01), Mickelson et al.
patent: 4675120 (1987-06-01), Martucci
patent: 5389496 (1995-02-01), Calvert et al.
patent: 5512200 (1996-04-01), Garcia
patent: 5567235 (1996-10-01), Carson et al.
patent: 5578347 (1996-11-01), Chan
patent: 5591989 (1997-01-01), Miyasaka et al.
Barr Michael
Beck Shrive P.
Diamond Seal, Inc.
LandOfFree
Glass coating cmposition and method of application does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Glass coating cmposition and method of application, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Glass coating cmposition and method of application will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1457059