ABSTRACT:
A pipe couple is shown for connecting two pipelines of different materials together in a well environment which prevents deterioration of the pipe due to galvanic action. The couple achieves its purpose by coating the interior of the more noble pipe section with a wear-resistant, non-conductive coating which prevents electrolytic action between the two dissimilar metals. It also achieves high pullout resistance while maintaining minimum outer dimensions to facilitate use of the couple in all types of wells including oil, gas and waste injection wells.

REFERENCES:
patent: 3186738 (1965-06-01), Dalrymple
patent: 3202562 (1965-08-01), Lang et al.
patent: 3620555 (1971-11-01), Hinds
patent: 4176033 (1979-11-01), Council
patent: 4345785 (1982-08-01), Bradford
patent: 4366971 (1983-01-01), Lula
patent: 4524996 (1985-06-01), Hunt
patent: 4600219 (1986-07-01), Yoshida
patent: 5069485 (1991-12-01), Allen et al.
patent: 5320388 (1994-06-01), Lacy et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Galvanic corrosion protection system does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Galvanic corrosion protection system, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Galvanic corrosion protection system will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-397838

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.