Metal founding – Process – Shaping liquid metal against a forming surface
Reexamination Certificate
2006-09-28
2010-12-07
Kerns, Kevin P (Department: 1793)
Metal founding
Process
Shaping liquid metal against a forming surface
C164S111000, C428S649000, C428S609000, C428S614000
Reexamination Certificate
active
07845388
ABSTRACT:
Magnesium or magnesium alloy components having galvanic corrosion protection isolators secured in place by metallurgical bonding during casting of the magnesium or magnesium alloy component. The isolators are formed of materials that are characterized by an absolute potential difference that is between that of magnesium and a contacting metallic component.
REFERENCES:
patent: 2011613 (1935-08-01), Brown et al.
patent: 2100257 (1937-11-01), Larson
patent: 4290868 (1981-09-01), Mack
patent: 4960296 (1990-10-01), Thelen et al.
patent: 5333913 (1994-08-01), Stallard
patent: 6659702 (2003-12-01), Kitayama et al.
patent: 6673469 (2004-01-01), Isaccsson et al.
patent: 6880940 (2005-04-01), Binfet
patent: 2006/0177683 (2006-08-01), Ballyns et al.
patent: 2001-246456 (2001-09-01), None
Luo Aihua A.
Sachdev Anil K.
Verbrugge Mark W.
GM Global Technology Operations Inc.
Kerns Kevin P
Reising Ethington P.C.
LandOfFree
Galvanic corrosion protection for magnesium components using... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Galvanic corrosion protection for magnesium components using..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Galvanic corrosion protection for magnesium components using... will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-4182504