Compositions – Electrolytes for electrical devices
Patent
1978-10-27
1980-07-22
Gantz, Delbert E.
Compositions
Electrolytes for electrical devices
204148, 252 39, 252 41, 252389R, 285 94, 585 10, C10M 124, C10M 318, C10M 118, C10M 312
Patent
active
042138680
ABSTRACT:
A coupling having dissimilar metal mating parts is provided with a grease comprising a hydrocarbon base oil containing a stearate gelling agent, particularly a Na, Li or Ba stearate. This coupling is anti-galvanic corrosive. Such couplings are useful in fire-fighting equipment where often aluminum and bronze components are in mating relationship, such as fire hose adaptors and hose nozzles.
REFERENCES:
patent: 1884749 (1932-10-01), Kocour
patent: 2240021 (1941-04-01), Rutherford
patent: 2533840 (1950-12-01), Roehner et al.
patent: 2810695 (1957-10-01), Young et al.
patent: 2827313 (1958-03-01), Conner
patent: 3069387 (1962-12-01), Allen et al.
patent: 3290244 (1966-12-01), Polishuk et al.
patent: 3939082 (1976-02-01), Williams et al.
Bitely, Jr. Clarence J.
Dromgold Luther D.
Murray, Jr. William S.
Friedman Morton
Gantz Delbert E.
Gazzola Albert L.
Vaughn Irving
Witco Chemical Corporation
LandOfFree
Galvanic corrosion prevention coupling does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Galvanic corrosion prevention coupling, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Galvanic corrosion prevention coupling will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2177630