ABSTRACT:
A coating composition for application to a metal part, which improves corrosion resistance and significantly reduces the co-efficient of friction of the surface of the part and a one coating step method for applying the coating to form two distinct layers on the coated part. The composition includes an oil phase in which polytetrafluoroethelene particles are suspended mixed with a resin film forming paint composition. Upon applying the coating to the part and curing of the resin film, the oil phase separates and forms a overlayer of oil having the polytetrafluoroethelene particles uniformly distributed in the oil layer.
REFERENCES:
patent: 3033808 (1959-01-01), Murray et al.
patent: 3438920 (1969-04-01), Halper et al.
patent: 3669728 (1972-06-01), Seiner
patent: 4284518 (1981-08-01), Reick
patent: 4284668 (1981-08-01), Nixon
Gira Gerald T.
Kinkelaar Edmund W.
Pekar Howard G.
Buscher Mark R.
Kremblas, Jr. Francis T.
Michl Paul R.
Texo Corporation
LandOfFree
Friction reducing coating for metal surfaces does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Friction reducing coating for metal surfaces, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Friction reducing coating for metal surfaces will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-171073