ABSTRACT:
A flux cored arc welding process for depositing a weld metal onto a revolving cylindrical workpiece. A weld deposit zone is moved along a longitudinal axis of the revolving cylindrical workpiece at a relative feed velocity of 1/32 to 2 inches per each revolution of the cylindrical workpiece, per each 0.1 foot to 2 feet per minute circumferential rate of revolution of the cylindrical workpiece. The weld deposit zone deposits a weld metal onto the revolving cylindrical workpiece in a spiral or helical fashion or manner.
REFERENCES:
patent: 2813190 (1957-11-01), Felmley, Jr.
patent: 2909649 (1959-10-01), Landis et al.
patent: 3075067 (1963-01-01), Axhelm
patent: 3611541 (1971-10-01), Garrett
patent: 4322596 (1982-03-01), Krakow et al.
patent: 4404450 (1983-09-01), Weldon
patent: 4782206 (1988-11-01), Ayres et al.
Owner's Manual by Miller Electric Mfg. Co., Mar. 1987.
Survey of Joining and Cutting Processes, pp. 5-11.
The Welding Handbook by American Welding Society, 1987, pp. 4.1-17 to 4.1-20, 5.4-1 to 5.4-2, & 6.3-2 to 6.3-12.
Carpenter John W.
Gulf Engineering Company, Inc.
Shaw Clifford C.
LandOfFree
Flux cored arc welding process does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Flux cored arc welding process, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Flux cored arc welding process will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-464294