ABSTRACT:
A method of fluidizing a cold lime-silica slag covering a molten metal. An acid flux is prepared from a particulate admixture of sodium fluoroaluminate and sodium silicate. The flux is mixed with the cold slag forming a fluid slag having at least 1% by weight F- and at least 1% by weight Na.sub.2 O. The treated slag has a reduced melting point allowing it to be mechanically skimmed from the molten metal and has a high sulfur capacity.

REFERENCES:
patent: 2757107 (1956-07-01), Heger et al.
patent: 3598170 (1971-08-01), Roberts
patent: 3721547 (1973-03-01), Dvorak
patent: 3982929 (1976-09-01), Heck et al.
patent: 3985546 (1976-10-01), Mrdjenovich
patent: 3998624 (1976-12-01), Harris
patent: 4126453 (1978-11-01), Heck
patent: 4147539 (1979-04-01), Kekish
patent: 4290809 (1981-09-01), Loane

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Fluidizing a lime-silica slag does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Fluidizing a lime-silica slag, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Fluidizing a lime-silica slag will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1741383

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.