ABSTRACT:
A suitable casting alloy for use in a fluid treatment device may be made as a copper-nickel-zinc-tin (CU--NI--ZN--SN) alloy without the addition of silver, silicon or magnesium, if certain identified trace metals are kept below certain levels. It appears that the previously identified additive metals, which are either expensive or dangerous, act to counteract the deleterious effects of these trace contaminants, and are not necessary of the contaminants are controlled. A method of forming the alloy prevents the explosive reactions encountered when melting together metals having significantly differing vaporization and melting temperatures.
REFERENCES:
patent: 3891394 (1975-06-01), Smith et al.
patent: 4429665 (1984-02-01), Brown
patent: 4632806 (1986-12-01), Morikawa et al.
patent: 4644674 (1987-02-01), Burrows et al.
patent: 5059217 (1991-10-01), Arroyo et al.
patent: 5124122 (1992-06-01), Wojcik
Understanding Copper Alloys, ed. Mendelhall, Olin Brass, 1977, pp. 3-5.
Norcross Alexander F.
Roy Upendra
LandOfFree
Fluid treatment alloy casting of Cu-Sn-Ni-Zn does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Fluid treatment alloy casting of Cu-Sn-Ni-Zn, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Fluid treatment alloy casting of Cu-Sn-Ni-Zn will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1328074