Flattened U-bolt and method

Metal treatment – Process of modifying or maintaining internal physical... – Heating or cooling of solid metal

Reexamination Certificate

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

C148S650000, C072S700000, C470S013000

Reexamination Certificate

active

06852181

ABSTRACT:
A method for cold forming a flattened, end-threaded rod into a U-bolt answers the need for high-strength steel rods that can be bent into flattened U-bolts by spring and suspension repair facilities or the like. By controlling the amount of work put into the end-threaded flattened rod during bending, it is possible to manufacture a flattened, end-threaded rod from a high-strength steel that can be successfully cold bent into a U-bolt. The amount or degree of flattening and the radius of the U-bolt are variables which applicant controls to successfully cold bend a high-strength steel flattened rod into a U-bolt. Therefore, the spring and suspension repair facility avoids the need to heat the flattened rods for warm forming and, instead, can maintain an inventory of end-threaded and flattened rods for cold forming into flattened U-bolt comply with OEM designs when modifying or repairing vehicles.

REFERENCES:
patent: 1862281 (1932-06-01), Schaefer
patent: 1900049 (1933-03-01), Ellison
patent: 2767836 (1956-10-01), Nachtman et al.
patent: 2767837 (1956-10-01), Nachtman et al.
patent: 2880855 (1959-04-01), Nachtman
patent: 2933424 (1960-04-01), Canney et al.
patent: 2953794 (1960-09-01), Klooz
patent: 3001897 (1961-09-01), Nachtman
patent: 3066408 (1962-12-01), Fader
patent: 3076361 (1963-02-01), Epstein et al.
patent: 3230118 (1966-01-01), Tufts
patent: 3488231 (1970-01-01), Zackay et al.
patent: 3488986 (1970-01-01), Stammbach
patent: 3557587 (1971-01-01), Cardillo
patent: 3573999 (1971-04-01), Gokyu
patent: 3668020 (1972-06-01), Lucht
patent: 3720087 (1973-03-01), Gottschlich
patent: 3877281 (1975-04-01), Shimizu et al.
patent: 3883371 (1975-05-01), Geary
patent: 3904445 (1975-09-01), Gallagher, Jr.
patent: 3908431 (1975-09-01), Jones et al.
patent: 3959999 (1976-06-01), Filatov et al.
patent: 4289548 (1981-09-01), Bucher et al.
patent: 4312210 (1982-01-01), Nishizawa et al.
patent: 4317355 (1982-03-01), Hatsuno et al.
patent: 4365824 (1982-12-01), Ohno et al.
patent: 4378687 (1983-04-01), Shilov et al.
patent: 4393679 (1983-07-01), Kusaba
patent: 4608851 (1986-09-01), Khare
patent: 4685319 (1987-08-01), Aoyagi et al.
patent: 4779439 (1988-10-01), Baldi
patent: 4805437 (1989-02-01), Heil, Jr. et al.
patent: 4958508 (1990-09-01), Lin
patent: 4966026 (1990-10-01), Nishino
patent: 4982591 (1991-01-01), McGahhey
patent: 5094698 (1992-03-01), Gallagher, Jr.
patent: 5121622 (1992-06-01), Kosak et al.
patent: 5203193 (1993-04-01), Iguchi et al.
patent: 5236520 (1993-08-01), Gallagher, Jr.
patent: 5287715 (1994-02-01), Kusaba
patent: 5330594 (1994-07-01), Gallagher, Jr.
patent: 5392624 (1995-02-01), Properzi
patent: 5453139 (1995-09-01), Gallagher, Jr.
patent: 5454888 (1995-10-01), Gallagher, Jr.
patent: 5496425 (1996-03-01), Gallagher, Jr.
patent: 5538566 (1996-07-01), Gallagher, Jr.
patent: 5704998 (1998-01-01), Gallagher, Jr.
patent: 6325874 (2001-12-01), Wheeler, Jr.
patent: 1535775 (1978-12-01), None
patent: 51144328 (1981-01-01), None
patent: 58027958 (1983-02-01), None
patent: WO 9315233 (1933-08-01), None
PCT/US 02/33893,International Search Report, Feb. 14, 2003.
C.W. Wegst,Stahlschlussel, 15th Edition, 1989.
C.I. Garcia, A.K. Lis and A.J. DeAdo,A New Cost-Effective Steel for High Strength Cold Forming Operations, 1988.
C.I. Garcia, A.K. Lis and A.J. DeArdo,A New Microalloyed Multi-phase Steel for High Strength Cold Heading Applications, Proceedings of the 60th Annual Convention and 1990 Division Meetings of the Wire Association International Inc., pp. 26-30.
Saarstahl,Wire and Wire Rods Hardened and Tempered in Coils, Brochure, Apr. 1981.
A.J. DeArdo,Accelerated Cooling: A Physical Metallurgy Perspective, Canadian Metallurgical Quarterly, vol. 27, No. 2, pp. 141-154, 1988.
R.G. Davies,The Deformation Behavior of a Vanadium-Strengthened Dual Phase Steel, Metallurgical Transactions, vol. 9A, pp. 41-52, Jan. 1978.
Isao Gokyu and Teruo Kishi,Warm Working of Steel, Japanese Inst. of Metal vol. 9, Supp. 1968.
M.L. Bernshtein and N.V. Filatova,Strengthening of Warm-Rolled Low-Carbon Steels, 2354 Metal Science and Heat Treatment 26, pp. 128-131, Feb. 1984.
Carl A. Keyser,Materials Science in Engineering, Second Edition, pp. 236-237, 1974, 2nd Edition.
Kobe Steel,High-Tensile Bolts, Chemical Abstracts No. 101411b, vol. 95 (Sep. 1981) No. 12, p. 219.
E. Nehl,Warm Extrusion of Free-Cutting Steels, CA 102(22): 888 63K American Chem Society, 604-8, 1984.
W.T. Lankford,Making, Shaping and Treating of Steel, 1985.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Flattened U-bolt and method does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Flattened U-bolt and method, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Flattened U-bolt and method will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-3447784

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.