Flame spray oxidation and corrosion resistant superalloys

Stock material or miscellaneous articles – All metal or with adjacent metals – Having metal particles

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

427405, 427423, 428553, 428564, 428652, 428656, 428667, 428668, 428678, 428937, B32B 1520

Patent

active

041017137

ABSTRACT:
A flame sprayed high energy milled powder coated article comprising a superalloy substrate and a coating consisting of chromium and at least one element selected from iron, cobalt or nickel. Optionally the coating can contain other elements, e.g., aluminum, carbon, yttrium or the rare earth elements.

REFERENCES:
patent: 3723092 (1973-03-01), Benjamin
patent: 3754903 (1973-08-01), Goward et al.
patent: 3864093 (1975-02-01), Wolfa
patent: 3873347 (1975-03-01), Walker et al.
patent: 3926568 (1975-12-01), Benjamin et al.
patent: 3961098 (1976-06-01), Bessen
patent: 3993454 (1976-11-01), Giggins, Jr. et al.
patent: 4005989 (1977-02-01), Preston

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Flame spray oxidation and corrosion resistant superalloys does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Flame spray oxidation and corrosion resistant superalloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Flame spray oxidation and corrosion resistant superalloys will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-340387

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.