ABSTRACT:
A fixture capable of a brittle pre-crack introduction of prescribed shape and size in a ceramic specimen with high reproducibility comprises an anvil provided on the upper side thereof with a central groove perpendicularly intersecting a specimen to be mounted thereon for pre-crack introduction and a groove for positioning the specimen and a platelike pusher possessing a smooth and flat lower surface. To ensure stability of the brittle pre-crack introduction, the positioning groove in the anvil is so formed as to rise rectangularly in an equal length on either side of the central groove and the overall length of the positioning groove, i.e. the sum of the lengths of the raised portions plus the width of the central groove, is kept from exceeding the length of the specimen. To enhance the results of the introduction, the lower surface of the pusher is finished with roughness of not more than 0.8S and flatness of not more than 0.01 mm.

REFERENCES:
patent: 3285060 (1966-11-01), Pessen
Sadahiro, Takeshi, Transverse Rupture Strength and Fracture Toughness of WC--Co Alloys, 1981, pp. 291-295.
Nose, Tetsuro and Fujii, Toshimitsu, Evaluation of Fracture Toughness for Ceramic Materials by a Single--Edged--Precracked--Beam Method, 1988, pp. 328-333.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Fixture for brittle pre-crack introduction in ceramic specimen does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Fixture for brittle pre-crack introduction in ceramic specimen, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Fixture for brittle pre-crack introduction in ceramic specimen will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1607997

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.