ABSTRACT:
A method for enhancing the mechanical properties of cast beryllium and beryllium alloy bodies by reducing beryllium grain size. More particularly, grain size is reduced by forming a metal beryllide phase that is soluble in molten beryllium but of limited solubility in the solid metal. Initially, molten beryllium is cast into a mold and solidified resulting in precipitation of the metal beryllide in the form of finely divided particles at the beryllium grain boundaries. The cast body is then mechanically worked below its recrystallization temperature to form an unstable, deformed microstructure which is converted to a fine grain microstructure during a subsequent anneal above the recrystallization temperature of the beryllium or beryllium alloy body. The anneal can be a separate operation or a continuation of the plastic deformation operation.

REFERENCES:
patent: 2872363 (1959-02-01), Macherey
patent: 3333994 (1967-08-01), Mallen et al.
patent: 3350241 (1967-10-01), Mallen et al.
patent: 3699798 (1972-10-01), Anderson, Jr. et al.
patent: 3791878 (1974-02-01), Taylor et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Fine grain beryllium bodies does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Fine grain beryllium bodies, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Fine grain beryllium bodies will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1279606

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.