Electrolysis: processes – compositions used therein – and methods – Electrolytic coating – Depositing predominantly single metal coating
Patent
1995-03-08
1996-07-23
Niebling, John
Electrolysis: processes, compositions used therein, and methods
Electrolytic coating
Depositing predominantly single metal coating
205253, 205101, C25D 322
Patent
active
055386172
ABSTRACT:
Incorporating an additive into a tin electroplating bath substantially inhibits soluble ferrous ions, ferric ions, and stannous ions from reacting thus minimizing the formation of stannic tin which is lost in the plating sludge.
REFERENCES:
patent: 2402185 (1946-06-01), Schweikher
patent: 2407579 (1946-09-01), Schweikher
patent: 2457152 (1948-12-01), Hoffman
patent: 2461507 (1949-02-01), Gray et al.
patent: 2512719 (1950-06-01), Hull
patent: 2585902 (1952-02-01), Gray
patent: 2736692 (1956-02-01), Eckert
patent: 2758075 (1956-08-01), Swalheim
patent: 3031400 (1960-05-01), Tsu
patent: 3518171 (1970-06-01), Merker et al.
patent: 3849263 (1974-11-01), Gedde
patent: 3887444 (1975-06-01), Fueki et al.
patent: 3907653 (1975-09-01), Horn
patent: 3915812 (1975-10-01), Yamagishi et al.
patent: 3926759 (1975-12-01), Horn et al.
patent: 4006213 (1977-02-01), Fisher et al.
patent: 4073701 (1978-02-01), Steinbicker et al.
patent: 4163700 (1979-08-01), Igarashi et al.
patent: 4329207 (1982-05-01), Maruta
patent: 4459185 (1984-07-01), Obata et al.
patent: 4702383 (1987-10-01), Babcock et al.
patent: 4717460 (1988-01-01), Nobel et al.
patent: 5006367 (1991-04-01), Lancsek
patent: 5094726 (1992-03-01), Nobel et al.
patent: 5108615 (1992-04-01), Hosea et al.
patent: 5110423 (1992-05-01), Little et al.
patent: 5118394 (1992-06-01), Makino et al.
patent: 5174887 (1992-12-01), Federman et al.
patent: 5178746 (1993-01-01), Darnall et al.
patent: 5185076 (1993-02-01), Yanada et al.
patent: 5296128 (1994-03-01), Gernon et al.
patent: 5298168 (1994-03-01), Guess
patent: 5378347 (1995-01-01), Thomson et al.
Fodor Edward S.
Steinbicker Richard N.
Yau Yung-Herng
Bethlehem Steel Corporation
Mayekar Kishor
Niebling John
LandOfFree
Ferrocyanide-free halogen tin plating process and bath does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Ferrocyanide-free halogen tin plating process and bath, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Ferrocyanide-free halogen tin plating process and bath will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-710603