ABSTRACT:
An FE--Ni--Cr-base superalloy consists essentially of, by weight, up to 0.15% C, up to 1.0% Si, up to 3.0% Mn, 30 to 49% Ni, 10 to 18% Cr, 1.6 to 3.0% Al, one or more elements selected from Groups IVa and Va whose amount or total amount is 1.5 to 8.0%, the balance being Fe, optionally, minor amounts of other intentionally added elements, and unavoidable impurities. The optional other elements which can be intentionally added to or omitted from the alloy include Mo, W, Co, B, Mg, Ca, Re, Y and REM. The superalloy is suitable for forming engine valves, knitted mesh supporters for exhaust gas catalyzers and the like, and has excellent high-temperature strength and normal-temperature ductility after long-time heating, as well as sufficient oxidation resistance properties for these uses.
REFERENCES:
patent: 3183084 (1965-05-01), Heydt et al.
patent: 3243287 (1966-03-01), Lillys et al.
patent: 3552950 (1971-01-01), Rundell et al.
patent: 3663213 (1972-05-01), Eiselstein et al.
patent: 4035182 (1977-07-01), Kowaka et al.
patent: 4172742 (1979-10-01), Rowcliffe et al.
patent: 4743318 (1988-05-01), Fischer et al.
patent: 4765956 (1988-08-01), Smith et al.
patent: 4767597 (1988-08-01), Nishinio et al.
patent: 5000914 (1991-03-01), Igarashi et al.
patent: 5137684 (1992-08-01), Fritzemeiar
Ohno Takehiro
Saka Tsutomu
Sato Katsuaki
Sato Koji
Hitachi Metals Ltd.
Honda Giken Kogyo Kabushiki Kaisha
Zimmerman John
LandOfFree
Fe-Ni-Cr-base superalloy, engine valve and knitted mesh supporte does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Fe-Ni-Cr-base superalloy, engine valve and knitted mesh supporte, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Fe-Ni-Cr-base superalloy, engine valve and knitted mesh supporte will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1987130