ABSTRACT:
An Fe-base superalloy essentially consisting of up to 0.20% C, up to 1.0% Si, up to 2.0% Mn, more than 25% and less than 30% Ni, 10 to 15% Cr, one or both of not less than 0.05% and less than 1.0% Mo and not less than 0.05% and less than 2.0% W so that an amount of Mo+0.5 W is not less than 0.05 and less than 1.0, 0.7 to 2.0% Al, 2.5 to 4.0% Ti, 0.05 to 1.0% Nb, and the balance being substantially Fe except impurities.
REFERENCES:
patent: 4165997 (1979-08-01), Smith, Jr. et al.
patent: 4377553 (1983-05-01), Korenko
Ohno Takehiro
Sato Koji
Hitachi Metals Ltd.
Yee Deborah
LandOfFree
Fe-base superalloy does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Fe-base superalloy, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Fe-base superalloy will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-212699