Alloys or metallic compositions – Nickel base – Chromium containing
Patent
1988-09-26
1992-06-23
Dean, R.
Alloys or metallic compositions
Nickel base
Chromium containing
148428, 420443, C22C 1905
Patent
active
051241234
ABSTRACT:
The present invention provides an alloy having improved crack growth inhibition and having high strength at high temperatures. The composition of the alloy is essentially as follows:
REFERENCES:
patent: 3046108 (1962-07-01), Eiselstein
Davis Jr. James C.
Dean R.
General Electric Company
Magee Jr. James
Rochford Paul E.
LandOfFree
Fatigue crack resistant astroloy type nickel base superalloys an does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Fatigue crack resistant astroloy type nickel base superalloys an, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Fatigue crack resistant astroloy type nickel base superalloys an will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-931617