ABSTRACT:
An improved eutectic superalloy composition is described. The eutectic composition upon solidification forms a gamma matrix, containing a substantial quantity of particles of the gamma prime phase, and containing about 12% by volume of aligned continuous chromium carbide fibers (Cr.sub.3 C.sub.2). Material of this composition is provided with significantly improved mechanical properties and surface stability through the addition of approximately one atomic percent of the material selected from the group consisting of manganese, technetium and rhenium. Directionally solidified articles of this composition have utility as gas turbine engine components.

REFERENCES:
patent: 3124452 (1964-03-01), Kraft
patent: 3554817 (1971-01-01), Thompson
patent: 3564940 (1971-02-01), Thompson et al.
patent: 3671223 (1972-06-01), Thompson et al.
patent: 3793010 (1974-02-01), Lemkey et al.
patent: 4012241 (1977-03-01), Lemkey
patent: 4111723 (1978-09-01), Lemkey
"The Influence of Off-Axis Reinforcement on the Tensile Strength of an Ni-Al-Cr-C Eutectic Composite", by G. J. May, Journal of Materials Science 10 (1975), 77-82.
"The Fatigue Behavior of an Aligned Ni-Al-Cr-C Eutectic Alloy", by G. J. May, Metallurgical Transactions, vol. 6A, May 1975.
"Creep Behavior of a Ni-Ni.sub.3 Al-Cr.sub.3 C.sub.2 Eutectic Composite", by Bullock et al., Acta Metallurgica, vol. 25, pp. 333-344, 1977.
"The Contribution of Fibre Reinforcement to the Tensile and Creep Strengths of .gamma.-.gamma.'-Cr.sub.3 C.sub.2 Eutectic Composite", by Miles et al., Published in the Proceedings of the Second Conference on In Situ Composites, 1976.
"Effects of Alloying Additions and High Rate Solidification on the Mechanical and Oxidation Behavior of the Directionally Solidified .gamma.-.gamma.'-Cr.sub.3 C.sub.2 Eutectic", by Bullock et al., Published in the Proceedings of the Third Conference on In Situ Composites, 1979.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Eutectic superalloy compositions and articles does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Eutectic superalloy compositions and articles, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Eutectic superalloy compositions and articles will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1613340

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.