ABSTRACT:
An erosion resistant protective structure for a turbine engine component comprises a shape memory alloy. The shape memory alloy includes nickel-titanium based alloys, indium-titanium based alloys, nickel-aluminum based alloys, nickel-gallium based alloys, copper based alloys, gold-cadmium based alloys, iron-platinum based alloys, iron-palladium based alloys, silver-cadmium based alloys, indium-cadmium based alloys, manganese-copper based alloys, ruthenium-niobium based alloys, ruthenium-tantalum based alloys, titanium based alloys, iron-based alloys, or combinations comprising at least one of the foregoing alloys. Also, disclosed herein are methods for forming the shape memory alloy onto turbine component.
REFERENCES:
patent: 4380574 (1983-04-01), Gessinger et al.
patent: 4832993 (1989-05-01), Coulon
patent: 4839245 (1989-06-01), Sue et al.
patent: 5448828 (1995-09-01), Willems et al.
patent: 5531369 (1996-07-01), Richman et al.
patent: 5956845 (1999-09-01), Arnold
patent: 6127044 (2000-10-01), Yamamoto et al.
patent: 6451454 (2002-09-01), Hasz et al.
patent: 6458317 (2002-10-01), Koskinen et al.
patent: 6607693 (2003-08-01), Saito et al.
patent: 7093423 (2006-08-01), Gowda et al.
patent: 2001/0021346 (2001-09-01), Doi et al.
patent: 2003/0194320 (2003-10-01), Villhard
patent: 2006/0068214 (2006-03-01), Gigliotti et al.
patent: 2551895 (1976-05-01), None
patent: 0 508 414 (1996-07-01), None
patent: 0 515 078 (1997-12-01), None
patent: 0 642 876 (2000-03-01), None
patent: 1054077 (2000-11-01), None
patent: 1054077 (2000-11-01), None
patent: 03036230 (1991-02-01), None
patent: 03150331 (1991-06-01), None
patent: WO-99/66102 (1999-12-01), None
patent: WO 99/66102 (1999-12-01), None
patent: WO-99/66102 (1999-12-01), None
Minoru Umemoto, “Nanocrystallization of Steels by Various Severe Plastic Deformation” Department of Production Systems Engineering, Toyohashi University of Technology, Toyohashi, Aichi 441-8580, Japan (Written in Jun. 2003), 10 pages.
http://www.wilkinsonsteel.com/Stainless/316.htm (Dec. 19, 2003) 2 pages.
T. Saito et al. “Multifunclional Alloys Obtained Via A Disclocation-Free Plastic Deformation Mechanism” Science, vol. 300 464-467 (Apr. 18, 2003).
U.S. Appl. No. 10/955,056, filed Sep. 30, 2004, Gigliotti, Jr. et al., Erosion And Wear Resistant Protective Structures For Turbine Components (available in IFW).
EPO Search Report dated Jun. 13, 2005.
Anand Krishnamurthy
Blank Jonathan Paul
Gigliotti, Jr. Michael Francis Xavier
Hardwicke Canan Uslu
Jiang Liang
Agosti Ann M.
Austin Aaron
Patnode Patrick K.
Zimmerman John J.
LandOfFree
Erosion and wear resistant protective structures for turbine... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Erosion and wear resistant protective structures for turbine..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Erosion and wear resistant protective structures for turbine... will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-3843870