ABSTRACT:
Cast iron alloy preferably of about 1.6 carbon, 2 nickel, 2 molybdenum, 28 chromium, and up to 1 of an additional element, balance substantially iron characterized by a matrix substantially entirely of tempered martensite with minimal retained austenite, containing ferrite phases and primary chromium-rich carbides with substantially no secondary carbides.
REFERENCES:
patent: 3961994 (1976-06-01), Thome
patent: 4043842 (1977-08-01), Joiret
patent: 4080198 (1978-03-01), Heyer et al.
patent: 4382828 (1983-05-01), Henych
Khandros Igor Y.
Larson Hugo R.
ABEX Corporation
Rutledge L. Dewayne
Yee Deborah
LandOfFree
Erosion and corrosion resistant cast iron alloy containing chrom does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Erosion and corrosion resistant cast iron alloy containing chrom, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Erosion and corrosion resistant cast iron alloy containing chrom will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-558861