Measuring and testing – Specimen stress or strain – or testing by stress or strain... – By loading of specimen
Patent
1980-05-30
1982-06-22
Ciarlante, Anthony V.
Measuring and testing
Specimen stress or strain, or testing by stress or strain...
By loading of specimen
73826, G01N 1908
Patent
active
043356150
ABSTRACT:
Equipment for testing materials for the effects of stress corrosion cracking, which includes more than two tensioning units, each consisting of a base plate, two guide bars, an upper and a lower cross-beam, a locking system for the guide of the lower cross-beam and a connecting flange between the cross-beam and a threaded bar for causing elongation of a test sample. The power drive supply block drives the threaded bar. A motor power unit is included in the power drive supply block and vertically-slippable gearing is inserted between the motor gearing and the block. The motor power unit consists of two stepping motors driving sun gears. The sun gears drive planetary gears which, by means of an arm, drive the drive shaft operatively associated with the threaded bar. In particular, the invention relates to equipment with six tensioning units comprising an automatic limit switch-off means and a lift system in the power drive supply block for separating the drive gears from the rest of the system. The angular speed of the stepping motors can be controlled by an electrically generated stepping frequency, the control unit, if desired, consisting of a microprocessor and a memory.
REFERENCES:
patent: 1485835 (1924-04-01), Bothezat et al.
patent: 1499546 (1924-07-01), Oxley
patent: 1877467 (1932-09-01), Lake
patent: 2185340 (1940-01-01), Howe
patent: 4030348 (1977-06-01), Fletcher et al.
Brunmayer Peter
Gellermann Siegfried
Kalfa Horst
Schubert Bruno
Ciarlante Anthony V.
DECHEMA
LandOfFree
Equipment for testing materials for stress corrosion cracking does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Equipment for testing materials for stress corrosion cracking, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Equipment for testing materials for stress corrosion cracking will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-648150