ABSTRACT:
The invention is directed to a process for preparing a sealant and adhesive useful, e.g., in double glazing systems. The sealant comprises 20-80 weight percent epoxidized natural rubber, 5-30 weight percent of at least one further epoxy compound, and, as a crosslinking agent, a polyamine or polymercaptan carrying trialkoxysilyl groups. The crosslinking agent is incorporated into the epoxidized natural rubber in one step.
REFERENCES:
patent: 2971864 (1961-02-01), Speier
patent: 4169822 (1979-10-01), Kutch et al.
patent: 4179537 (1979-12-01), Rykowski
patent: 4328277 (1982-05-01), Molari, Jr.
patent: 4369222 (1983-01-01), Hedrick et al.
patent: 4416923 (1983-11-01), Murase
patent: 4444936 (1984-04-01), Schwarz et al.
patent: 4463129 (1984-07-01), Shinada et al.
Blank Norman
Duck Edward W.
Reich Karl
Jaeschke Wayne C.
Looper Valerie E.
Sellers Robert E.
Szoke Ernest J.
Teroson GmbH
LandOfFree
Epoxidized natural rubber with epoxy resin and trialkoxysilyl gr does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Epoxidized natural rubber with epoxy resin and trialkoxysilyl gr, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Epoxidized natural rubber with epoxy resin and trialkoxysilyl gr will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-192689