ABSTRACT:
Quench cracking of nickel base superalloy articles is avoided by plating the articles with a layer of nickel or similar metal prior to heat treatment.

REFERENCES:
patent: 1859623 (1932-05-01), Gregg
patent: 1934741 (1933-11-01), Schulein
patent: 1953445 (1934-04-01), Stevens
patent: 2295777 (1942-09-01), Denneen et al.
patent: 2619439 (1952-11-01), Rennick
patent: 2887420 (1959-05-01), Llewelyn
patent: 3037878 (1962-06-01), Cowles et al.
patent: 3250650 (1966-05-01), Gray
patent: 3370993 (1968-02-01), Carpenter et al.
patent: 3489540 (1970-01-01), Cook
patent: 3558367 (1971-01-01), Eck
patent: 3741821 (1973-06-01), Athey et al.
patent: 4253885 (1981-03-01), Maurer et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Elimination of quench cracking in superalloy disks does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Elimination of quench cracking in superalloy disks, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Elimination of quench cracking in superalloy disks will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2211287

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.