Electrostatic enrichment of trona and nahcolite ores

Chemistry of inorganic compounds – Treating mixture to obtain metal containing compound – Alkali metal

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

23302T, 209127R, 209127A, 209128, 209214, C22B 2610, B03C 700, B03C 100, C01D 3124

Patent

active

043754546

ABSTRACT:
Calcined trona and/or nahcolite bearing ore particles are separated into a plurality of fractions of relatively uniform particle size. Those calcined particles smaller than about 6.7 mm in size and larger than about 0.2 mm in size are passed through an electrostatic separator to obtain an ore concentrate containing a greater percentage of soda ash and a lesser percentage of insoluble impurities than were present in the ore; a middling fraction and an ore tailing fraction containing a lesser percentage of soda ash and a greater percentage of insoluble impurities than were present in the ore. The middling fraction may be recycled to increase the yield of ore concentrate. Calcined particles smaller than about 0.2 mm may be combined with the ore concentrate. The combined ore concentrate fraction may be marked as technical grade soda ash or used as a high grade feed to a monohydrate refining process.

REFERENCES:
patent: 1872591 (1932-08-01), Hoeman
patent: 2765074 (1956-10-01), Diamond
patent: 2832469 (1958-04-01), Lawver
patent: 2839190 (1958-06-01), Lawver
patent: 3244476 (1966-04-01), Smith
patent: 3458039 (1969-07-01), Singewald
patent: 3477566 (1969-11-01), Autenrieth et al
patent: 3479133 (1969-11-01), Warzel
patent: 3480139 (1969-11-01), Fricke et al.
patent: 3493109 (1970-02-01), Carta et al.
patent: 3760941 (1973-09-01), Singewald et al.
patent: 3819805 (1974-06-01), Graves et al.
patent: 3821353 (1974-06-01), Weichman
patent: 3941685 (1976-03-01), Singewald et al.
patent: 3962403 (1976-06-01), Wyslouzil
patent: 4341744 (1982-07-01), Brison et al.
Perry, R. H. et al. Chemical Engineers Handbook, 5th Edition McGraw-Hill Book Co., NY. NY., 1973 pp. 21-62-21-65.
Faas, F. Electrostatic Separation of Granular Materials Bureau of Mines Bulletin #603, 1962, 155 pages.
Faas, Foster, Effect of Temperature on the Electrostatic Separation of Mineral Bureau of Mines Report of Investigation, Apr. 1966, 5213.
The Chemical Age, Metalurgical Section, Applied Electrostatic Separation Efficient Ore Dressing Technique, pp. 235-239, Sep. 1943.
H. B. Johnson, Selective Electrostatic Separation, Mining Technology Jan. 1938. A IMME TP 877.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Electrostatic enrichment of trona and nahcolite ores does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Electrostatic enrichment of trona and nahcolite ores, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Electrostatic enrichment of trona and nahcolite ores will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1460026

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.