Electroluminescent phosphor and its production method

Compositions – Inorganic luminescent compositions – Zinc or cadmium containing

Reexamination Certificate

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

Reexamination Certificate

active

07135130

ABSTRACT:
The invention provides electroluminescent phosphor having superior luminance and a long life. The host material is ZnS.aAO, of which “A” is at least one element selected from among magnesium (Mg), calcium (Ca), strontium (Sr), and barium (Ba). “a” ranges from 0.001 to 0.01. Either one of or both copper (Cu) or manganese (Mn) is contained as an activator. At least one element selected from among chlorine (Cl), bromine (Br), iodine (I), and aluminum (Al) is contained as a co-activator. The luminance and life span of the electroluminescent phosphor can be increased by limiting “a”, which represents the proportion of alkaline earth metal oxide (AO) introduced into the zinc sulfide, within the range of 0.001 to 0.01.

REFERENCES:
patent: 07-090262 (1995-04-01), None

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Electroluminescent phosphor and its production method does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Electroluminescent phosphor and its production method, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Electroluminescent phosphor and its production method will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-3656445

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.