ABSTRACT:
The tensile elongation of a tungsten-nickel-iron alloy containing essentially 95 weight percent reprocessed tungsten, 3.5 weight percent nickel, and 1.5 weight percent iron is increased from a value of less than about 1 percent up to about 23 percent by the addition of less than 0.5 weight percent of a reactive metal consisting of niobium and zirconium.
REFERENCES:
patent: 2793951 (1957-05-01), Green et al.
patent: 3177076 (1965-04-01), Timmons et al.
patent: 3307982 (1967-03-01), Milligan et al.
Properties of Tungsten and Tungsten Alloys for Reactor Shielding Applicats, Watts, AEC Report Y-1675, Jun. 1969, pp. 8, 9, 15 & 17.
Carlson Dean F.
Hamel Stephen D.
Larcher Earl L.
Steiner Arthur J.
The United States of America as represented by the Department of
LandOfFree
Ductile tungsten-nickel-alloy and method for manufacturing same does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Ductile tungsten-nickel-alloy and method for manufacturing same, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Ductile tungsten-nickel-alloy and method for manufacturing same will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-562690