Ductile duplex iron-based alloy containing aluminum

Specialized metallurgical processes – compositions for use therei – Processes – Free metal or alloy reductant contains magnesium

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

75128G, 75128T, 148 37, C22C 3840

Patent

active

044989288

ABSTRACT:
A two-phase ductile iron-based alloy which is resistant to oxidation and fidation at high temperatures is disclosed. The alloy contains from about 8 to 20 wt % of Cr; about 6 to 30 wt % of Ni; about 3 to 11.5 wt % of Al; and 0 to 2 wt % of Mo; about 0 to 1 wt % of Si; about 0 to 2 wt % of Mn; about to 0 to 0.1 wt % of C; about 0 to 0.02 wt % of S; about 0 to 0.02 wt % of P; about 0 to 1 wt % of Ti; about 0 to 2 wt % of Nb and Ta; and the balance of Fe. The atomic ratio of nickel to aluminum is between 0.8 and 1.2.

REFERENCES:
patent: 1941648 (1934-01-01), Armstrong
patent: 4204862 (1980-05-01), Kado et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Ductile duplex iron-based alloy containing aluminum does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Ductile duplex iron-based alloy containing aluminum, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Ductile duplex iron-based alloy containing aluminum will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1388083

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.