ABSTRACT:
Cast superalloys of the formula P.sub.x Q.sub.y R.sub.z wherein P is an element selected from the group consisting of Fe, Ni, Cr, Co or mixtures thereof, wherein Q is a refractory element selected from the group consisting of Mo, W, Ta or a mixture thereof wherein R is a reactive element selected from the group consisting of Al, Ti, Cb or mixtures thereof, x is from about 65 to about 95 atomic percent, y is from about 1 to about 10 atomic percent, z is from about 1 to about 18 atomic percent and x+y+z is equal to about 100 in the form of thin foil are made ductile by the presence of appreciable amounts of amorphous phase and micro-crystalline, metastable single phase and subsequently boron is deposited as nickel, iron or cobalt boride on the surface of the foil at a temperature below the crystallization temperature of the superalloy. Such foil is especially suited for preplacement in a joining operation such as brazing.

REFERENCES:
patent: 3753794 (1973-08-01), Paulon et al.
patent: 4052201 (1977-10-01), Polk et al.
patent: 4056411 (1977-11-01), Chen et al.
patent: 4059441 (1977-11-01), Roy et al.
patent: 4067732 (1978-01-01), Roy
patent: 4116682 (1978-09-01), Polk et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Ductile brazing foil for cast superalloys does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Ductile brazing foil for cast superalloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Ductile brazing foil for cast superalloys will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-739503

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.