This invention relates to the directional solidification of superalloys, in particular nickel-based superalloys, by imposition of a predetermined temperature profile in the solidification front and, depending on the desired results, a predetermined rate of advance of said solidification front, whereas castings of markedly superior fatigue resistance are produced.
REFERENCES:
patent: 2229866 (1940-01-01), Munro
patent: 2875483 (1959-03-01), Hughes
patent: 3124452 (1964-03-01), Kraft
patent: 3495649 (1970-02-01), Waters
patent: 3515546 (1970-06-01), Greenewald
patent: 3669180 (1972-06-01), Moore
patent: 3770047 (1973-11-01), Kirkpartick
patent: 3842895 (1974-10-01), Mehrabian
patent: 4033401 (1977-07-01), Wlodawer
patent: 4057097 (1977-11-01), Lux
patent: 4175609 (1979-11-01), El Gammal et al.
patent: 4318753 (1982-03-01), Anderson
patent: 4411713 (1983-10-01), Betts
patent: 4434014 (1984-02-01), Smith
patent: 4540038 (1985-09-01), Burke
patent: 4717432 (1988-01-01), Ault
Alter Wendy S.
Hamilton William D.
Schmidt Deborah D.
Lin Kuang Y.
Manning John R.
Seemann Jerry L.
Sheehan William J.
The United States as represented by the Administrator of the Nat
LandOfFree
Directional solidification of superalloys does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Directional solidification of superalloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Directional solidification of superalloys will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-760194