ABSTRACT:
A relatively high surface area electrode is provided which can be utilized as an anode for extended periods of time without replacement in an electrolytic reaction in which oxygen is evolved. The anode of the present invention comprises a carbonaceous fibrous material (e.g. a fabric, tow, or felt) which bears a surface coating of a mixed crystal material consisting essentially of ruthenium oxide and titanium oxide. The anode is particularly suited for usage in the removal of harmful contaminants (i.e. organic or inorganic contaminants) from waste streams even when present in relatively low concentrations.
REFERENCES:
patent: 3071637 (1963-01-01), Horn et al.
patent: 3072558 (1963-01-01), Myers et al.
patent: 3214647 (1965-10-01), Louzos et al.
patent: 3446607 (1969-05-01), Volk et al.
patent: 3459917 (1969-08-01), Felts
patent: 3471383 (1969-10-01), Tiedemann
patent: 3476604 (1969-11-01), Faber
patent: 3619382 (1971-11-01), Lupinski
patent: 3632498 (1972-01-01), Beer
patent: 3637468 (1972-01-01), Icxi et al.
patent: 3723150 (1973-03-01), Druin et al.
patent: 3754457 (1973-08-01), Erlichmann
patent: 3759805 (1973-09-01), Chapman et al.
patent: 3764499 (1973-10-01), Okubo et al.
patent: 3775520 (1973-11-01), Ram et al.
patent: 3811943 (1974-05-01), Minck et al.
patent: 3818082 (1974-06-01), Burns et al.
patent: 3827964 (1974-08-01), Okubo et al.
patent: 3829327 (1974-08-01), Omori et al.
patent: 3852113 (1974-12-01), Yokota et al.
patent: 3859187 (1975-01-01), Druin et al.
patent: 3894884 (1975-07-01), Druin et al.
patent: 3900556 (1975-08-01), Clarke
patent: 3915822 (1975-10-01), Veltman
patent: 3923629 (1975-12-01), Shaffer
patent: 3925524 (1975-12-01), Kimmel et al.
patent: 3953313 (1976-04-01), Levenson
patent: 3954950 (1976-05-01), Ram et al.
patent: 4040918 (1977-08-01), Johnson et al.
patent: 4046663 (1977-09-01), Fleet et al.
patent: 4046664 (1977-09-01), Fleet et al.
patent: 4061557 (1977-12-01), Nishizawa et al.
patent: 4108754 (1978-08-01), Fleet et al.
patent: 4108755 (1978-08-01), Fleet et al.
patent: 4108757 (1978-08-01), Fleet et al.
patent: 4112140 (1978-09-01), Heikel et al.
patent: 4235695 (1980-11-01), DeNora et al.
Reger Arie
Sprague B. Sheldon
Celanese Corporation
Edmundson F.
LandOfFree
Dimensionally stable high surface area anode comprising graphiti does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Dimensionally stable high surface area anode comprising graphiti, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Dimensionally stable high surface area anode comprising graphiti will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1878044