ABSTRACT:
Complete coating or localized repair and replacement of a diffusion aluminide coating applied to the surface of an article is attained through use of a powdered Fe-Al alloy as a source of aluminum. In another aspect, more accurate control of a coating method, such as for aluminide diffusion coating, is achieved when a source powder is provided in a layer, such as a tape, preferably by combining the powder with a binder which decomposes substantially without residue upon heating.

REFERENCES:
patent: 3149996 (1964-09-01), Wagner et al.
patent: 3415676 (1968-12-01), Nishi et al.
patent: 3513013 (1970-05-01), Willis et al.
patent: 3589935 (1971-06-01), Brill-Edwards et al.
patent: 3598638 (1971-08-01), Levine
patent: 3647497 (1972-03-01), Levine et al.
patent: 3667985 (1972-06-01), Levine et al.
patent: 3837901 (1974-09-01), Seybolt
patent: 3847649 (1974-11-01), Sova

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Diffusion coating method does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Diffusion coating method, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Diffusion coating method will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-73102

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.