Metal fusion bonding – Process – Diffusion type
Patent
1985-03-05
1986-09-30
Ramsey, Kenneth J.
Metal fusion bonding
Process
Diffusion type
228198, 22826313, 228119, B23P 604, B23K 104
Patent
active
046142967
ABSTRACT:
A diffusion brazing process for superalloy parts is performed on the one hand by the interposition between the pieces to be joined of a joining layer having a composition close to that of the parts and containing a "fluxing" element, which renders it more readily meltable, and on the other hand, a heat treatment effecting the brazing by the melting of the joining layer and its resolidification, by the diffusion of the flux. The process of the invention is characterized, particularly in view of permitting the use of a joining layer of a greater thickness than that of the layers used in the known diffusion brazing processes, in that said joining layer consists of a mixture of a superalloy powder and an alloy powder containing the flux.
REFERENCES:
patent: 2714760 (1955-08-01), Boam et al.
patent: 3108861 (1963-10-01), Cape
patent: 3496630 (1970-02-01), Duff et al.
patent: 3574924 (1971-04-01), Dibble
patent: 3678570 (1972-07-01), Paulonis et al.
patent: 3692501 (1972-09-01), Hoppin et al.
patent: 4005988 (1977-02-01), Paulonis et al.
patent: 4008844 (1977-02-01), Duvall et al.
patent: 4285459 (1981-08-01), Baladjanian et al.
patent: 4299629 (1981-11-01), Haack
patent: 4381944 (1983-05-01), Smith, Jr. et al.
Duvall, D. S. et al., "TLP Bonding: A New Method for Joining Heat Resistant Alloys," Welding Journal, Apr. 1974, pp. 203-214.
Sims, Chester T. et al., editors, "The Superalloys: Vital High Temperature Gas Turbine Materials for Aerospace and Industrial Power," 1972, pp. 596-597.
Ramsey Kenneth J.
Societe Nationale d'Etude et de Construction de Moteurs d'Aviati
LandOfFree
Diffusion brazing process for pieces of superalloys does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Diffusion brazing process for pieces of superalloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Diffusion brazing process for pieces of superalloys will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-980236