ABSTRACT:
A sensor for a heat flux differential scanning calorimeter in which the differential temperatures are measured between locations external to the regions of heat exchange between the sensor and sample containers. The measured differential temperatures respond to the magnitude of the heat flow rate between the sensor and the sample and reference containers and are rendered insensitive to variations in the magnitude and distribution of thermal contact resistance between the sensor and the containers.
REFERENCES:
patent: 3554002 (1971-01-01), Harden et al.
patent: 4095453 (1978-06-01), Woo
patent: 5033866 (1991-07-01), Kehl et al.
patent: 5224775 (1993-07-01), Reading et al.
patent: 5288147 (1994-02-01), Schaefer et al.
patent: 5439291 (1995-08-01), Reading
patent: 5711604 (1998-01-01), Nakamura
patent: 5788373 (1998-08-01), Huetter et al.
patent: 5842788 (1998-12-01), Danley et al.
patent: 6431747 (2002-08-01), Danley
patent: 6488406 (2002-12-01), Danley
patent: 6508585 (2003-01-01), Nakamura et al.
patent: 6530686 (2003-03-01), Nakamura
patent: 6583391 (2003-06-01), Jorimann et al.
patent: 6641300 (2003-11-01), Lacey et al.
patent: 7371006 (2008-05-01), Schick
patent: 2003/0072348 (2003-04-01), Danley
patent: 2003/0165179 (2003-09-01), Danley
G.W.H. Hohne, W. Hemminger, H.J. Flammersheim, “Differential Scanning Calorimetry”, Springer, Berlin, 1996, pp. 21-40.
R.L. Danley, “New Heat Flux DSC Measurement Technique”, Elsevier, Thermochimica Acta 395 (2003), pp. 201-208.
S.L. Boersma, “A Theory of Differential Thermal Analysis And New Methods of Measurement and Interpretation”, Journal of The American Ceramic Society, Delft, Holland, 1955, vol. 38, No. 8, pp. 281-284.
A. Savitzky, M.J.E. Golay “Smoothing and Differentiation of Data by Simplified Least Squares Procedures”, Analytical Chemistry, Connecticut, Jul. 1964, vol. 36, No. 8, pp. 1627-1639.
A. Savitzky, M.J.E. Golay, “Comments on Smoothing and Differentiation of Data by Simplified Least Square Procedure”, Analytical Chemistry vol. 44, No. 11, Sep. 1972, pp. 1906-1909.
Baghdadi Aslan
Jagan Mirellys
Paul Hastings Janofsky & Walker LLP
Verbitsky Gail
Waters Investments Limited
LandOfFree
Differential scanning calorimeter sensor and method does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Differential scanning calorimeter sensor and method, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Differential scanning calorimeter sensor and method will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-4035008