ABSTRACT:
Porous and non-porous compositions include diamond particles, non-diamond particles, or mixtures of particles consolidated with polycrystalline diamond. The composite compositions of the present invention may be formed by a process which includes the steps of preforming the particles into a preform having a desired shape, and consolidating the preform with polycrystalline diamond. The polycrystalline diamond is preferably formed using CVD techniques including application of sufficient microwave energy to maintain the preform at a temperature of between about 670.degree. and 850.degree. C. The preform may be rotated during a portion of the deposition process.

REFERENCES:
patent: 4104441 (1978-08-01), Fedoseev et al.
patent: 4960643 (1990-10-01), Lemelson
patent: 5015528 (1991-05-01), Pinneo
patent: 5077102 (1991-12-01), Wagner et al.
patent: 5187021 (1993-02-01), Vydra et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Diamond film and solid fiber composite compositions does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Diamond film and solid fiber composite compositions, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Diamond film and solid fiber composite compositions will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1247701

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.