Stock material or miscellaneous articles – Web or sheet containing structurally defined element or... – Including a second component containing structurally defined...
Patent
1994-10-20
1997-03-11
Turner, A. A.
Stock material or miscellaneous articles
Web or sheet containing structurally defined element or...
Including a second component containing structurally defined...
428408, 4283044, 4283122, 4283179, 4283184, 4283191, B32B 900
Patent
active
056099550
ABSTRACT:
Porous and non-porous compositions include diamond particles, non-diamond particles, or mixtures of particles consolidated with polycrystalline diamond. The composite compositions of the present invention may be formed by a process which includes the steps of preforming the particles into a preform having a desired shape, and consolidating the preform with polycrystalline diamond. The polycrystalline diamond is preferably formed using CVD techniques including application of sufficient microwave energy to maintain the preform at a temperature of between about 670.degree. and 850.degree. C. The preform may be rotated during a portion of the deposition process.
REFERENCES:
patent: 4104441 (1978-08-01), Fedoseev et al.
patent: 4231762 (1980-11-01), Hara et al.
patent: 4925701 (1990-05-01), Jansen et al.
patent: 4987002 (1991-01-01), Sakamoto et al.
Crystallume
Turner A. A.
LandOfFree
Diamond film and mixed diamond and non-diamond particle composit does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Diamond film and mixed diamond and non-diamond particle composit, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Diamond film and mixed diamond and non-diamond particle composit will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-441880