Diamond coated cutting member and method of making the same

Cutting by use of rotating axially moving tool – Tool having crystalline cutting edge

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

407119, 408224, 761086, B23B 2720

Patent

active

057161704

ABSTRACT:
A diamond coated elongate rotary cutting member and method of making the same. The cutting member includes an axially forward cutting surface, a flute and a fluted land. The cutting member comprises a substrate with hard grains bonded together with a metallic binder. The substrate has a first substrate region that presents an irregular surface so as to define the axially forward cutting surface and the fluted land. The first substrate region contains relatively large hard grains near the surface thereof that are larger in size than the hard grains in the interior of the substrate. A diamond coating is on the surface of the first substrate region. The substrate has a second substrate region that defines the flute.

REFERENCES:
patent: Re34180 (1993-02-01), Nemeth et al.
patent: 4282289 (1981-08-01), Kullander et al.
patent: 4374685 (1983-02-01), Suzuki et al.
patent: 4636252 (1987-01-01), Yoshimura et al.
patent: 4643620 (1987-02-01), Fujii et al.
patent: 4690691 (1987-09-01), Komanduri
patent: 4731296 (1988-03-01), Kikuchi et al.
patent: 4755399 (1988-07-01), Fujii et al.
patent: 4762445 (1988-08-01), Bunting et al.
patent: 4843039 (1989-06-01), Akesson et al.
patent: 4966501 (1990-10-01), Nomura et al.
patent: 4985070 (1991-01-01), Kitamura et al.
patent: 4990403 (1991-02-01), Ito
patent: 5020394 (1991-06-01), Nakamura et al.
patent: 5022801 (1991-06-01), Anthony et al.
patent: 5028451 (1991-07-01), Ito et al.
patent: 5066553 (1991-11-01), Yoshimura et al.
patent: 5068148 (1991-11-01), Nakahara et al.
patent: 5071294 (1991-12-01), Suzuki et al.
patent: 5096736 (1992-03-01), Anthony et al.
patent: 5100703 (1992-03-01), Saijo et al.
patent: 5123217 (1992-06-01), Ishikawa et al.
patent: 5137398 (1992-08-01), Omori et al.
patent: 5178645 (1993-01-01), Nakamura et al.
patent: 5204167 (1993-04-01), Saijo et al.
patent: 5273557 (1993-12-01), Cerutti et al.
patent: 5326195 (1994-07-01), Brox
patent: 5370944 (1994-12-01), Omori et al.
patent: 5380408 (1995-01-01), Svensson
patent: 5391422 (1995-02-01), Omori et al.
patent: 5585176 (1996-12-01), Grab et al.
JIS B 0601 (1882) "Definitions and Designation of Surface Roughness", JIS Handbook 1989 Tools, Japanese Standards Association (1989), pp. 2245-2255.
ANSI B 46.1-1978, "Surface Texture" ASME (1978), pp. 1-37.
"Surface Texture and Roundness Measurement Handbook", Sheffield Measurement Division, Warner L& Swasey (1988), pp. 47-48.
McCune et al., "An Auger Electronic Spectroscopy Study of the Surface of Ni-Mo Cemented Ti(CN) Substrates Used for Deposition of Crystalline Diamond Particles," Surface & Coatings Technology, 39/40 (1989), pp. 223-233.
75th Autumn Congress of the Light Metal Society, Nov. 1988, Katsumura et al., "Effect of Co Content in the Substrate Material and of the Surface State of the Substrate on the Performance of a Diamond-Coated Sintered Hard Alloy Tool in Cutting Al-18% Si Alloy", pp. 2-8.
Jindal et al., "Adhesion Measurements of Chemically Vapor Deposited and Physically Vapor Deposited Hard Coatings on WC-CO Substrates", Thin Solid Films 154 (1987) pp. 361-375.
Kikuchi et al., "Diamond Coated Inserts: Characteristics and Performance", Applications of Diamond Films and Related Materials, Ed. by Tzeng et al., (1991) pp. 61-68.
Murakawa et al., "Chemical Vapour Deposition o a Diamond Coating onto a Tungsten Carbide Tool Using Ethanol", Surface and Coatings Technology, 36 (1988), pp. 303-310.
Saito et al., "Adhesion Strength of Diamond Film on Cemented Carbide Insert", Diamond and Related Materials, 2 (1993), pp. 1391-1395.
Haubner et al., "Diamond Growth by Hot-Filament Chemical Vapor Deposition: State of the Art," Diamond and Related Materials, 2 (1993) pp. 1277-1294.
Yarbrough et al., "The Chemical Vapor Deposition of Diamond", Materials Science Forum, vols. 52 and 53 (1989), pp. 151-174.
Saijo et al., "The Improvement of the Adhesion Strength of Diamond Films", Surface and Coatings Technology, 43/44 (1990), pp. 30-40.
Lux et al., "Low Pressure Synthesis of Superhard Coatings", Intl. J. Ref. Met. & Hard Mater., 8 (1989), pp. 158-174.
Kuo et al., "Adhesion and Tribological Properties of Diamond Films on Various Substrates", J. Mater. Res., vol. 5, No. 11, Nov. 1990, pp. 2515-2523.
Soderberg et al., "Factors Influencing the Adhesion of Diamond Coatings on Cutting Tools", Vacuum, vol. 41, Nos. 4-6 (1990), pp. 1317-1321.
Park et al., "Behavior of Co Binder Phase during Diamond Deposition on WC-Co Substrate", Diamond and Related Materials, 2 (1993), pp. 910-917.
Saito et al., "Application of Diamond Films from CO-H.sub.2 Plasma to Tool Blade Coating", Journal of Materials Science, 26, (1991), pp. 2937-2940.
Nesladek et al., "Improved Adhesion of CVD Diamond Films To Steel and Wc-Co Substrates", Diamond And Related Materials, 3 (1993), pp. 98-104.
"Metals Handbook Ninth Edition", vol. 7, Powder Metallurgy (1984), pp. 385-388, 398.
Tulhoff, "On the Grain Growth of WC in Cemented Carbides", Modern Developments in Powder Metallurgy, ed. by Hausner et al., vol. 14, Special Materials (1981), pp. 269-279.
Gaser, "Edge and Surface Honing on Various Shaped PCD & cBN Inserts", SME Technical Paper MR92-357 (1992).
Schneider, "Edge Grinding and Radiusing with Superabrasives", MAN, Sep. 1992, pp. 46-47.
Hosomi et al., "Diamond CVD Researches as Patent Applied", Applications of Diamond Films and Related Materials, ed. by Tzeng et al., Proceedings of Auburn University Conference, Aug. 1991, Elsevier Science Publishers B.V., (1991), pp. 15-24.
Israelsson, "A Progress Report on Cutting Tool materials", American Machinist, Dec. 1992, pp. 39, 40.
"Advanced Cutting Tool Materials", Kennametal Catalogue No. A90-67 (1988), pp. 1, 2, 77-86, 94-98, 101 and 102.
"Standard Test Method for Apparent Porosity in Cemented Carbides", ASTM Designation, B276-86.
"American National Standard for Cutting Tools--Indexable Inserts--Identification System", ANSI B212.4-1986.
Eastman et al., "Machining MMCs", Cutting Tool Engineering, Oct. 1993, pp. 38, 40-44.
Scheider,, "Precision Edge Radius Grinding of Diamond Cutting Tools and Inserts", SME Technical Paper MR91-195 (1991).
Scheider, "New Abrasive Edge and Surface Preparation Tools, Techniques and Technology for Fabricated Material Applications", SME Technical Paper FC91-426 (1991).
Craig, Phillip, Senior Editor, "Thin-Film-Diamond Derby", Cutting Tool Engineering, vol. 44, No. 1, Feb. 1992, Reprinted by Crystallume Engineered Diamond Products (6 pages).
Mason, Frederick, "Diamond: the Material of the Future", American Machinist, Feb. 1990, pp. 43-46.
Crystallume Engineered Diamond Products Brochure, "Engineering CVD Diamond for Extraordinary Performance in Demanding Applications", (1991) (7 pages).
Yagi, Masaru, "Cutting Performance of Diamond Deposited Tool on Al-18 mass%Si Alloy", Science and Technology of New Diamond, edited by S. Saito, O. Fukunaga and M. Yoshikawa, pp. 399-404, copyright by KTK Scientific Publishers, Terra Scientific Publishing Company, 1990.
Shibuku, Kunio; Yagi, Masaru; Saijo, Kosuke; and Takatsu, Sokichi, "Adhesion Strength of Diamond Films on Cemented Carbide Substrates", Surface and Coatings Technology, 36 (1988) 295-302.
M. Yagi et al., "Cutting Performance of Diamond Cutting Tool for A1-18 mass% Si Alloy", Journal of Japan, Institute of Light Metals, vol. 39, No. 6, pp. 417-422 (1989) (Trans. and Orig. Japanese).
Katsumura et al., "The Effects of Cobalt Content and Surface State of Substrate on Cutting Performance of Diamond Deposited Cemented Carbide Tool for Al-18% Si Alloy", Journal of Japan, Institute of Light Metals, vol. 39, No. 9, pp. 634-638 (1989) (Trans. and Orig. Japanese).
Saijo et al., "The Tool Life of Diamond Coatings in Milling an Al-Si Alloy, Applications of Diamond Films and Related Materials", ed. by Tzeng et al., Elsevier Sci. Pub. B.V. (1991), pp. 69-76.
Suzuki et al., "Diamond Deposition on WC-Co Cemented Carbide by Hot Filament Method", J. Jpn. Soc. Powder Metall., 33 (5) (1986) (English translation and Japanese language copy (pp. 38-45).

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Diamond coated cutting member and method of making the same does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Diamond coated cutting member and method of making the same, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Diamond coated cutting member and method of making the same will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2072348

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.