ABSTRACT:
A devolatilized room temperature vulcanizable silicone rubber composition comprising a silanol polymer, a plasticizing fluid, a cross-linking agent, a curing promoter and optionally, a filler wherein the plasticizing fluid and the silanol polymer are devolatilized prior to being mixed to form the room temperature vulcanizable silicone rubber composition by heating them at temperatures of at least 200.degree. C. under vacuum for at least 5 minutes. If there is utilized a filler and the filler is treated with cyclopolysiloxanes or silazanes, then preferably the filler is also devolatilized.
REFERENCES:
patent: 3382205 (1968-05-01), Beers
patent: 3635743 (1972-01-01), Smith
patent: 3813364 (1974-05-01), De Zuba et al.
patent: 4153501 (1979-05-01), Fink et al.
patent: 4250290 (1981-02-01), Peterson
Briggs Sr. Wilbert J.
General Electric Company
Koltos E. Philip
LandOfFree
Devolatilized room temperature vulcanizable silicone rubber comp does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Devolatilized room temperature vulcanizable silicone rubber comp, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Devolatilized room temperature vulcanizable silicone rubber comp will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-947334