ABSTRACT:
A determination of the temper quality of a tempered glass sheet is made which includes determining the percentages of the thickness of a tempered glass sheet which are in compression as well as the sheet's tensile membrane stress. The process uses a CO.sub.2 laser beam, either on a painted or unpainted glass sheet, to shatter the glass sheet and then comparing the number of pulses required for the glass sheet to shatter to a correspondence, e.g., a graph, of tensile membrane stress v. compression layer thickness as a % of the total thickness of the glass sheet.

REFERENCES:
patent: 3543979 (1970-12-01), Grove et al.
patent: 3808439 (1974-04-01), Remois
patent: 3811775 (1974-05-01), Abu-Saud
patent: 4655589 (1987-04-01), Cestaro et al.
patent: 4697082 (1987-09-01), Bartelsen
patent: 5254149 (1993-10-01), Hashemi et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Determination of tensile membrane stress and compressive layer t does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Determination of tensile membrane stress and compressive layer t, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Determination of tensile membrane stress and compressive layer t will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-349688

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.