ABSTRACT:
Apparatus and methods for monitoring localized or pitting corrosion of metal or other material are described. A probe having a working electrode made of the same material as the material being monitored is located in the same corroding environment as the material being monitored. The electrochemical noise detected between the working electrode and other electrodes is processed to provide an indication of the state of localized corrosion of the material being monitored. An anodic bias voltage is applied to the working electrode. This bias voltage accentuates localized corrosion at the working electrode, improving sensitivity and permitting more accurate evaluation of the electrochemical noise signals.
REFERENCES:
patent: 3766042 (1973-10-01), Wilson
patent: 4056445 (1977-11-01), Gauntt et al.
patent: 4351703 (1982-09-01), Winslow
patent: 5139627 (1992-08-01), Eden et al.
U. Bertocci et al, J. Electrochem. Soc., vol. 14, No. 1, (Jan. 1997) pp. 31-43. Noise Resistance Applied to Corrosion Measurement.
Martinchek Gregory A.
Yaffe Max R.
Gamry Instruments, Inc.
McNeil Jennifer
Tung T.
LandOfFree
Detection of pitting corrosion does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Detection of pitting corrosion, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Detection of pitting corrosion will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-560677