ABSTRACT:
A method is disclosed for the deoxidation of open type steels, e.g. rimmed and capped steels, which are particularly useful in the production of sheet products with improved formability. The requisite amount of deoxidation in the ladle is achieved through the use of conventional deoxidizers, other than aluminum (preferably silicon carbide). Deoxidation in the mold is also achieved without the use of aluminum. Here, however, it is necessary that mold deoxidation be achieved through the use of magnesium, generally added in the form of a magnesium-nickel alloy.

REFERENCES:
patent: 3754893 (1973-08-01), Frawley
patent: 3801303 (1974-04-01), Kotler
patent: 3885956 (1975-05-01), Obst

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Deoxidation of open type steels for improved formability does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Deoxidation of open type steels for improved formability, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Deoxidation of open type steels for improved formability will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-546913

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.