ABSTRACT:
A process for the deoxidation of a refractory metal containing minor concentrations of oxygen is disclosed. In this process the refractory metal is contacted with a metallic deoxidant in a dry, inert atmosphere. The metallic deoxidant and the refractory metal are heated to at least liquefy the metallic deoxidant and at least partially deoxidize the refractory metal. The refractory metal is thereafter cooled and contaminants on its surface are removed.
REFERENCES:
patent: 2537068 (1951-01-01), Lilliendahl et al.
patent: 2653869 (1953-09-01), Gregory et al.
patent: 2834667 (1958-05-01), Rostron
patent: 4126493 (1978-11-01), Wurm
patent: 4519837 (1985-05-01), Down
patent: 4923531 (1990-05-01), Fisher
Lechert Jr. Stephen J.
RMI Titanium Company
LandOfFree
Deoxidation of a refractory metal does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Deoxidation of a refractory metal, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Deoxidation of a refractory metal will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-780941