ABSTRACT:
The present invention provides a method for improving aluminum alloy plate product properties by delaying final stretching of the plate product. During processing of the product, a time interval or intentional delay is provided between the final cold rolling step and the final stretching step. By delaying the final stretching procedure, an aluminum alloy plate product is provided with an improved fracture toughness without significant decrease in strength values. The method of intentionally delaying final stretching is particularly adapted for 2000 series aluminum alloys.
REFERENCES:
patent: 4294625 (1981-10-01), Hyatt et al.
patent: 4808248 (1989-02-01), Ozelton et al.
Biddison Alan M.
Dean R.
Koehler Robert R.
Reynolds Metals Company
LandOfFree
Delaying final stretching for improved aluminum alloy plate prop does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Delaying final stretching for improved aluminum alloy plate prop, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Delaying final stretching for improved aluminum alloy plate prop will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1540144