ABSTRACT:
The invention provides continuously-cast product free of ambient atmosphere contaminants and free of nonmetal solid entrapment. Methods and apparatus are provided for flow of molten metal from ladle to tundish to mold machine, free of contact with ambient atmosphere; and, tundish slag cover is removed, by discharge of a nonreactive gas to provide a selected limited surface area of tundish metal, which is free of slag cover, for insertion of a ladle shroud to deliver molten metal, free of entrapment of nonmetal slag cover, for continuous casting. Transitional casts, before clean metal is obtainable with each new ladle of molten metal, are eliminated; and the duration of uninterrupted continuous casting of clean metal is extended.

REFERENCES:
patent: 3469740 (1969-09-01), Crowe
patent: 5232046 (1993-08-01), Gallucci et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Decreasing contamination of molten metal prior to solidification does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Decreasing contamination of molten metal prior to solidification, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Decreasing contamination of molten metal prior to solidification will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1206311

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.