ABSTRACT:
A process for removing layers of paint or other non-metallic coatings from a coated metal hanger or the like comprising the steps of freezing the coating to embrittle it and shrink it toward the metal hanger, heating the metal hanger without heating the coating to expand the metal toward the coating, and stressing the coating by said expanding and shrinking to break and fragment the coating and cause it to fall off the metal hanger.
REFERENCES:
patent: 3337815 (1974-09-01), Bixby
patent: 3934379 (1976-01-01), Braton et al.
patent: 3948679 (1976-04-01), Lewis
patent: 4205530 (1980-06-01), Soecknick et al.
Brodbeck Howard D.
Burckhardt Klaus A.
A. Earley John F.
A. Earley III John F.
Cohen Sharon T.
Metz Andrew
MG Industries, Inc.
LandOfFree
Debonding process for removing non-metallic coatings from metal does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Debonding process for removing non-metallic coatings from metal , we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Debonding process for removing non-metallic coatings from metal will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1066153