ABSTRACT:
A method for inhibiting the corrosion of martensitic and ferritic stainless steel surfaces which are exposed to hot carbonate solutions which comprises contacting said stainless steel surfaces with nickel ions and preferably with at least 10 ppm of nickel ion contained in the hot alkali metal carbonate solution.
REFERENCES:
patent: 2957762 (1960-10-01), Young
patent: 3024201 (1962-03-01), Bregman
patent: 3079220 (1963-02-01), Boes et al.
patent: 3151087 (1964-09-01), Ryznar et al.
patent: 3625888 (1971-12-01), Redmore et al.
patent: 3699052 (1972-10-01), Petrey et al.
patent: 3721526 (1973-03-01), Foroults et al.
patent: 3738806 (1973-06-01), Feiler
patent: 3901651 (1975-08-01), Benner et al.
patent: 3951844 (1976-04-01), Mago
Durling Robert Edward
Gancy Alan Brian
Allied Chemical Corporation
Garris Bradley
Rooney Gerard P.
Stewart Anthony J.
Wolk Morris O.
LandOfFree
Corrosion inhibition of stainless steel exposed to hot carbonate does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Corrosion inhibition of stainless steel exposed to hot carbonate, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Corrosion inhibition of stainless steel exposed to hot carbonate will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2086289