Metal treatment – Stock – Copper base
Patent
1998-12-16
2000-10-24
Yee, Deborah
Metal treatment
Stock
Copper base
420470, C22C 902
Patent
active
061361038
ABSTRACT:
A copper-tin-titanium alloy which consists of 12 to 20% by weight tin, 0.002 to 1% by weight titanium, remainder copper and usual impurities. It is possible to add further elements. Semifinished products made from the copper alloy according to the invention are preferably produced by thin-strip casting or spray compacting. Due to a particularly advantageous combination of high mechanical strength properties with excellent ductility, combined with good resistance to corrosion, semifinished products made from the copper alloy according to the invention have numerous possible uses.
REFERENCES:
patent: 5004581 (1991-04-01), Takagi et al.
patent: 5102621 (1992-04-01), Sara
Boegel Andreas
Hansmann Stephan
Hofmann Uwe
Mueller Hilmar R.
Riedle Joachim
Wieland-Werke AG
Yee Deborah
LandOfFree
Copper-tin-titanium alloy does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Copper-tin-titanium alloy, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Copper-tin-titanium alloy will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1959643